MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified

Material Notes: Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.

Features: High temperature performances; Excellent dimensional stability
Typical Applications: Appliances handles; Spotlight; Electrical components

Information provided by Bieglo Gmbh for Lavergne Performance Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 123 MPa5 mm/min; ASTM D638
Elongation at Break 3.6 %5 mm/min; ASTM D638
Flexural Strength 182 MPa1.3 mm/min; ASTM D790
Flexural Modulus 8000 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 84.3 J/m
@Temperature 23.0 °C
ASTM D256
 
Processing PropertiesOriginal ValueComments
Feed Temperature 245 - 260 °C
Middle Barrel Temperature 250 - 265 °C
Front Barrel Temperature 255 - 270 °C
Nozzle Temperature 260 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 65.0 - 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
RTP Company RTP 4603 HI FR  Syndiotactic Polystyrene (SPS) Glass Fiber 20% - High Impact - Flame Retardant
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester
E-Polymers TEKAMID® TB110SG30 30% Glass Fiber Reinforced, High Impact PA6 Resin
Lavergne VYPET VNT 1020 Polyester-PC Alloy

PLAVER917 / 150644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.