MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese 193 LDPE polymer for adhesives, automotive and compounds
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: 193 resin is suitable for use in hot melt adhesive and coating applications. It complies with Code of Federal Regulation 21 CFR Section 177.1520 subject to extraction limitations for specific end use applications. Additives:

Applications: Adhesives & Sealants; Automotive

Information provided by Celanese Corporation.

Key Words: hot melt coating and adhesive applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9115 g/ccAT Plastics PTM-03
Melt Flow 400 g/10 min
@Load 0.325 kg,
Temperature 125 °C
Modified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Tensile Strength at Break 7.50 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 110 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 0.125 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 99.0 °CDSC; ASTM D3417
Ring & Ball Softening Point 109 °CASTM E28
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO)
Zylog Hipolyene® 3152 MC Thermoplastic Polyolefin & PP Compound
Celanese 280 LDPE polymer for adhesives and molding

PATEVB20 / 25976

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.