MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Norton® Tygon® R-3603 Laboratory and Vacuum Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Replaced by Tygon® S3 E-3603. Description: Tygon® R-3603: Crystal-clear and flexible, Tygon® Laboratory Tubing handles virtually all inorganic chemicals found in the lab. It is non-oxidizing and non-contaminating. Long-lasting and crack-resistant, Tygon® Laboratory Tubing is less permeable than rubber tubing. The glassy-smooth inner bore helps prevent buildup so that cleaning is facilitated. Coils are marked at 1-foot intervals for easy measuring. Autoclavable. Remains flexible at -45°F (-43°C). Durometer hardness: Shore A, 55.

Features/Benefits:
  • Outstanding chemical resistance
  • Lot-to-lot consistency for reproducible results
  • Increases productivity in peristaltic pumps -- outlasts other clear tubing 2 to 1
  • Standard sizes available to hold full vacuum at room temperature
  • Smooth, polished inner wall
  • Non-aging and non-oxidizing
  • Meets FDA CFR Part 175.300 Criteria
Typical applications include General Laboratory, Analytical Instruments, Peristaltic and Vacuum Pumps, Ideal for Condensers, Incubators, Desiccators, Gas Lines and Drain Lines.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792-91
Water Absorption 0.24 %24 hours at 23°C; ASTM D570-81
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5515 seconds; ASTM D2240-91
Tensile Strength, Yield 1650 psiASTM D412-92
Elongation at Break 450 %ASTM D412-92
100% Modulus 0.650 ksi
@Strain 100 %
ASTM D412-92
Tear Strength 125 pliInitial Tear Strength; ASTM D624-91 Die B
Compression Set 61 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 107 %ASTM D412-92
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 608 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -58.0 °FASTM D746-79
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
LNP STARAMIDE PM-3603 HI 012 BK846 Polyamide 6, Mineral Filler
Dow Silastic® 1604-T SILICONE RUBBER
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems

PSTGQZ190 / 68704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.