MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Sika Sikasil® WS-295 FPS Neutral cure, field pigmentable silicone sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Sikasil-WS 295 FPS sealant is a field pigmentable, no bleed, one component plus color pack, non-sag elastomeric, neutral cure silicone sealant for use in most common weatherproofing applications on a wide variety of materials. Meets the requirements of ASTM C-920, Type S, Grade NS, Class 50, Use NT, M, G, A, O; TT-S-00230C, Type II, Class A; CAN/CGSB-19.13-M87, AAMA 802.3 Type II, AAMA 803.3, AAMA 805.2, AAMA 808.3

Where to Use: Sikasil-WS 295 FPS silicone sealant has been specifically designed for:

  • As a weatherseal in nonstructural glazing applications including gap, toe and heel beads
  • As a weatherseal in glass to glass butt joint glazing.
  • Sealing expansion and control joints in precast concrete panels and metal curtain walls.
  • Perimeter sealing of doors, windows and other building components.
  • Adhering stiffeners to building panels.
  • Excellent for use in unitized curtain wall systems.
Advantages:
  • One-part plus color pack
  • Unaffected by most atmospheric conditions
  • Non-staining
  • Joint movement ±50%
  • Excellent adhesion
  • Excellent gunnability in all temperatures

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 37 g/l
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM C661
Tensile Strength 200 psiASTM D412
Tensile Stress at Strain 55.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 700 %ASTM D412
Peel Strength 30.0 plion aluminum, glass and concrete; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -80.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 168 - 336 hourASTM C679
Tack-Free Time 50.0 min
Working Life 20.0 - 30.0 minTool/Work Time (Initial Skin)
Shelf Life 12.0 Month
@Temperature <=27.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorsWhite, Colonial White, Aluminum, Limestone, Black, Bronze, Medium Bronze

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA949 / 209856

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.