MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cellulose Acetate Butyrate (CAB) Film
Categories: Polymer; Film; Thermoplastic; Cellulosic

Material Notes: Ultra Clear cellulose acetate butyrate film, low shrinkage, additive free, pinhole free; can be formulated with additives. Information typical of products used for flexible electronics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 13.0 - 76.0 microns
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 88.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Melting Point 235 °C
Shrinkage 1.0 %
 
Optical PropertiesOriginal ValueComments
Haze 0.83 %
Gloss 138 %
Transmission, Visible 94.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
AGC F-Clean® GR
Evonik Trogamid® CX9701 Transparent Nylon
Mitsui TPX® DX820 Methylpentene Copolymer
Dow HV 1520/40

PFLEXSM03 / 179519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.