MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Renishaw 6091 Vacuum casting resin
Categories: Polymer; Thermoset

Material Notes: Description: Simulates ABS

Features: UV stable

Suitable for: Lenses, optical applications

Information provided by Renishaw

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccPart B
 1.10 g/ccPart A
Viscosity 160 cPPart B
 800 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
@Temperature 80.0 °C
Cured; ISO 868
 81
@Temperature 23.0 °C
Cured; ISO 868
 81
@Temperature 60.0 °C
Cured; ISO 868
Tensile Strength 58.9 MPaCured; ISO R 527
Elongation at Break 11 %Cured; ISO R 527
Tensile Modulus 2220 MPaCured; ISO R 527
Flexural Strength 101 MPaCured; ISO 178
Flexural Modulus 2835 MPaCured; ISO 178
Izod Impact, Notched (ISO) 7.30 kJ/m²Cured; ISO 180
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.208 W/m-KCured; ISO BS 874
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CCured, (test piece 110 mm × 12.7 mm × 6.4 mm); ISO 75
Shrinkage 0.70 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.515
Transmission, Visible 99.7 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 °CResin Temp
Mold Temperature 70.0 - 75.0 °C
Cure Time 120 - 150 min
@Temperature 70.0 °C
Pot Life 460 sec
@Load 0.100 kg
 
Descriptive Properties
ColorColorless
Diffused lights0.07
Mixing ratio by weightA:B
Paralleled lights93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Renishaw SG95 Vacuum casting resin
Renishaw SG95-LP Vacuum casting resin
Renishaw 8060-1 Vacuum casting resin
Renishaw 8052 Vacuum casting resin
Phillips Sumika Marlex® RGC-020-04 Polypropylene; Random Copolymer

PRENISH020 / 206383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.