MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCAL™ 80 Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akrocal 80 is a dispersion of a fine particle size calcium oxide in a naphthenic binder. It has the consistency of putty.

General Recommendations: Akrocal 80 is used at levels of 5.0 to 10.0 parts per 100 of rubber. As a moisture scavenger, Akrocal provides protection against blistering and porosity. Addition of this product should be towards the end of a single pass mix or during the second pass. One variable important in determining the use level of Akrocal is the time of the year. Those months which bring high humidity in a plant may require larger amounts of Akrocal to provide the protection needed to produce acceptable product. The filler loading and type of filler, as well as the mixing procedure, are also important factors.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.21 g/cc
Particle Size 6.56 µmMedian
Particle Mesh Size 325 Mesh<1.0% (typical)
 
Thermal PropertiesOriginal ValueComments
Melting Point 180 - 189 °CEVA Bags
 
Descriptive Properties
Active0.8minimum CaO
AppearanceOff White
BinderNaphthenic Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH120 / 315038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.