MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Rolling Oil ISO Grade 320
Categories: Fluid; Lubricant

Material Notes: Rolling Oil is a high-quality, multipurpose rolling oil developed for rolling non-ferrous metals, such as aluminum, brass, copper and copper alloys. It also is recommended for use as a bearing lubricant, hydraulic oil and roll-coating oil in many mill applications. Rolling Oil is formulated to provide excellent oxidation resistance, wear protection, protection against rust and corrosion, and resistance to foaming. It has excellent water-separating properties to minimize the formation of emulsions. It is nonstaining to aluminum and yellow metals.

Applications:

  • Hot rolling of non-ferrous metals
  • Circulating oil for plain and rolling-element bearings in mill applications
  • Hydraulic oil in mill applications
  • Roll-coating oil in many mill applications
Rolling Oil meets the requirements of the following industry and OEM specifications:
  • U.S. Steel 127, 136
  • Vickers (Eaton) I-286-S
Features/Benefits:
  • Excellent oxidation resistance and thermal stability
  • Excellent wear protection for gears and bearings
  • Protects against rust and corrosion
  • Nonstaining to non-ferrous metals
  • Excellent water-separating properties
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/cc
Density 7.41 lb/gal
Viscosity Measurement 96Index
Saybolt Viscosity at 100°F 1649 SUS
Saybolt Viscosity at 210°F 118 SUS
Kinematic Viscosity at 40°C (104°F) 310 cSt
Kinematic Viscosity at 100°C (212°F) 23.7 cSt
Oxidative Stability 10 hourRPVOT; ASTM D2272
 5000 hourTOST; ASTM D943-04a
ASTM Color 2.5ASTM D1500
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.420 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °C
Flash Point 304 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401
FZG Scuffing Test>12 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphor bronze 5% Sn, UNS C51000, OSO50 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO70 Temper flat products

WCON5222 / 198475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.