MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gadolinium, Gd
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.89 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 157.251995
Atomic Number 64
X-ray Absorption Edge 0.2468 ÅK
 1.4787 ÅLI
 1.56081 ÅLII
 1.70955 ÅLIII
Electronegativity 1.2Pauling
Ionic Radius 0.938 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 37polycrystalline
Tensile Strength, Ultimate 190 MPa
Tensile Strength, Yield 173 MPa
Elongation at Break 37 %
Tensile Modulus 54.8 GPa
Bulk Modulus 37.9 GPa
Poissons Ratio 0.259
Shear Modulus 21.8 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000131 ohm-cm
Magnetic Susceptibility 0.00226cgs/g
Curie Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 98.5 J/g
CTE, linear 9.40 µm/m-°C
@Temperature 100 °C
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 8.80 W/m-K
Melting Point 1310 - 1312 °C
Boiling Point 3273 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.337
@Wavelength >=645 nm,
Temperature 1025 - 1313 °C
 
Component Elements PropertiesOriginal ValueComments
Gadolinium, Gd 100 %
 
Descriptive Properties
CAS Number7440-54-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked
Erbium, Er
Gold, Au
Americium, Am

AMEGd00 / 39

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.