MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SMAC SMACTANE® SP Damping Material
Categories: Other Engineering Material

Material Notes: A viscoelastic rubber material developed by SMAC for space applications and maximizes the damping properties in a wide range of temperatures & frequencies

Damping properties:

  • Damping properties are determined by visco-analysis
  • The damping criteria is given by the loss angle tangent (also called Tangent or loss factor). It is a function of frequency and temperature

    Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Outgassing - Total Mass Loss 0.0079 %0.0079 %RML
 0.0088 %0.0088 %TML
Collected Volatile Condensable Material 0.00020 %0.00020 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 42 - 5242 - 52NFT 46-052
Tensile Strength 10.9 MPa1580 psiNF T 46-002
Elongation at Break 800 %800 %NF T 46-002
 840 %840 %Shear; NF T 46-023
100% Modulus 0.710 MPa
@Strain 100 %
103 psi
@Strain 100 %
NF T 46-002
Shear Modulus 0.000410 GPa
@Strain 100 %
0.0595 ksi
@Strain 100 %
NF T 46-023
Shear Strength 6.60 MPa957 psiNF T 46-023
 
Descriptive Properties
Delta Tangent (G"/G')0.20 Hz @ 20°C
 0.651.00E+06 Hz @ 20°C
 0.7100 Hz @ 20°C
 1.14000 Hz @ 20°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SMAC SMACTANE® 60 1114S- N01 Damping Material
SMAC SMACTANE® 70 1114S- N04 Damping Material
SMAC SMACTANE® 50 1114S- N03 Damping Material
SMAC SMACMOUNT® 2150S Damping Material
SMAC SMACSIL® 1114S- S02 Damping Material

PZSMAC039 / 146155

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.