MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott BOROFLOAT® Borosilicate Float Glass
Categories: Ceramic; Glass; Optical; Oxide; Silicon Oxide

Material Notes: This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting from the float glass process opens up new applications for borosilicate flat glass in laboratories, chemical process plants and in the home appliance and lighting industries.

BOROFLOAT® flat glass is highly resistant to water; neutral, acidic and saline solutions; as well as to chlorine, bromine, iodine and organic substances. Even over long periods of time and at high temperatures that exceed 100°C, BOROFLOAT® exceeds the chemical resistance of most metals and other materials.

Information provided by SCHOTT North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.23 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 480HK 0.1/20; E DIN/ISO 9385
Modulus of Elasticity 63.0 GPa
Poissons Ratio 0.20
Shear Modulus 26.3 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.10e+6 ohm-cm
@Temperature 350 °C
 1.00e+8 ohm-cm
@Temperature 250 °C
Dielectric Constant 4.6
@Frequency 1e+6 Hz
Dielectric Strength 16.0 kV/mm50 Hz
Dissipation Factor 0.0037
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.25 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.830 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 1.12 W/m-K
@Temperature 90.0 °C
Maximum Service Temperature, Air 450 °CLong Term, depends on temperature gradient
 500 °CShort Term, depends on temperature gradient
Transformation Temperature, Tg 530 °C
Softening Point 815 °C107.6 dPa-s
Annealing Point 560 °C1013 dPa-s
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.463
@Wavelength 1014 nm
IR Hg
 1.472
@Wavelength 588 nm
nd
 1.481
@Wavelength 435.8 nm
Blue Hg
 1.489
@Wavelength 365 nm
UV Hg
Abbe Number 65.41ve
Optical Dispersion 0.00719nF - nC
Transmission, Visible 92 %
@Thickness 0.700 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Pyrex® 7740 Borosilicate Glass Sheet
Borosilicate Glass, Low Expansion
Schott N-BK7 Glass
Borosilicate Glass
Schott MEMpax® Borosilicate Glass

CSGT0001 / 1986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.