MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics MRI FS-85V Pre-Fired Refractory Shapes
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: MRI pressed fired shapes are used in a variety of alloy melt-pour systems. The pressed manufacture process meets the tight tolerance specifications required by end users. Precise size dies and detailed product inspection provide the user with a high-quality, dimensionally accurate refractory shape.

MRI FS-85V 85% fused silica mix, ideal for extreme thermal shock conditions and ferrous/nonferrous metal contact.

Features:

  • Variety of available compositions in high alumina and fused silica.
  • Extreme tight tolerance capabilities
  • Low gas permeability to ferrous alloys
  • Good non-wetting characteristics
  • Excellent mechanical strength
  • Proven performance in super alloy, investment
  • Applications:

  • Standard size crucibles and liners for induction melting and investment casting
  • Tundish nozzles - meet user demands on pour stream and pour speeds
  • Gas atomized nozzles - for custom-designed atomizing powder metal systems
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Bulk Density 1.747 g/cc
    Porosity 22 %Apparent
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.510 ksi
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 3.20 µin/in-°F
    @Temperature 20.0 °C
    Thermal Conductivity 10.6 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    ASTM C417
    Maximum Service Temperature, Air 2750 °F
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 14 %
    Alkalis 0.45 %
    CaO+MgO 0.15 %
    Fe2O3 0.30 %
    SiO2 85 %
    TiO2 0.70 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Borosilicate Glass
    Chosun Refractories SM-A Special Mortar for Sliding Gate Valve
    Morgan Advanced Ceramics Kaowool® Wet Felt Thermal Ceramic
    Morgan Advanced Ceramics Cerox® FS-85V Thermal Ceramic
    Thermal Ceramics Kaowool HS Low Temperature Board

    CTHERM148 / 2468

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.