MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.

Application examples: Thin stretch film for food packaging, coextrusion, cling film.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.935 g/cc0.935 g/ccISO 1183
Vinyl Acetate Content 14 %14 %
Thickness 40.0 microns1.57 milfor samples tested on this data sheet
 15.0 - 100 microns0.591 - 3.94 milpossible range, depending on extrusion conditions
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 6.50 MPa943 psiISO 527-3
Film Tensile Strength at Yield, TD 4.90 MPa711 psiISO 527-3
Film Elongation at Break, MD 370 %370 %ISO 527-3
Film Elongation at Break, TD 650 %650 %ISO 527-3
Modulus of Elasticity 0.0620 GPa8.99 ksiISO 527-2
Elmendorf Tear Strength, MD 3.70 g/micron94.0 g/milISO 6383-2
Elmendorf Tear Strength, TD 4.50 g/micron114 g/milISO 6383-2
Dart Drop Test 300 g0.662 lbISO 7765-1
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-3
Film Tensile Strength at Break, TD 23.0 MPa3340 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 °C194 °FISO 11357
Vicat Softening Point 68.0 °C154 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ISO 14782
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 170 °C284 - 338 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
Dow Elvax® 440 Ethylene Vinyl Acetate
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade)

PTOTAL707 / 130432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.