MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel Superplast® SP300 Prehardened Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Superplast® 300 (SP300) is a prehardened steel with a BHN 300 (32 HRC) to be used for plastic injection molds, extrusion dies, and compression molds offering improved performance for the mold maker as well as the mold user. For a similar level of mechanical properties (wear resistance), this grade provides an easier and more reliable machinability than conventional steels (P20/W1.2311).

This improvement is the result of a new chemical balance (lower carbon content and micro alloy additions) and a better microstructure. The homogeneity of the plate or block is improved compared to conventional steels, such as P20/W1.2311 which may be subject to hard spots.

SP300 is designed to provide an improved weldability and machinability compared to P20/W1.2311. It is more compatible with finishing operations such as polishing and chemical etching. SP300 may open some new opportunities through the possibility of weld repairs allowing for design changes during manufacturing or production.

SP300 is designed for use at 300 HB. If hardness is lost during the mold making process (by heating the steel to a temperature above 525°C (977°F), the original mechanical properties can be recovered by following a full cycle heat treatment.

SP300 is well adapted to machining, (drilling or milling), with high speed steel as well as carbide tools. Its machinability is better than that of conventional P20. It ranks between the machinability of DIN grades W1.2311 (low sulfur) and W1.2312 (resulfurized). It can be machined using the same parameters as P20 with a much longer tool life, or increased feeds and speeds will enable a significant increase in productivity.

Composition notes: Typical values for a 100 mm (4") thick plate. Boron is also present.

Information provided by BICO Akron, Inc., a subsidiary of Groupe Arcelor.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 290 - 320Guaranteed in the range 290 - 320 HB for thickness 20 mm to 600 mm.
Hardness, Rockwell C 32
Tensile Strength, Ultimate 1020 MPa
Tensile Strength, Yield 920 MPa
Elongation at Break 13.5 %
Modulus of Elasticity 205 GPaYoungs Modulus
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc -15.0 Oe
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°C
@Temperature 20.0 - 100 °C
 12.4 µm/m-°C
@Temperature 20.0 - 200 °C
 12.8 µm/m-°C
@Temperature 20.0 - 300 °C
 13.1 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 40.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 %
Chromium, Cr 1.3 %
Iron, Fe 97 %As remainder
Manganese, Mn 1.3 %
Molybdenum, Mo 0.40 %
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
International Mold Steel NAK-HH Precipitation Hardened Mold Steel
ASTM A485 Steel, Grade 4
AISI Type O7 Tool Steel
ASTM A485 Steel, Grade 2
International Mold Steel NAK55 Precipitation Hardened Mold Steel

NINDUST00 / 17538

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.