MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo GLAMIDE® T-663G50A MXD66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade T-663G50A is a GF reinforced, aromatic MXD66 nylon. It has a good appearance and contains 50% GF.

50

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccAbsolute Drying; ASTM-D792
Filler Content 50 %50 %
Water Absorption 0.30 %0.30 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 0.80 %0.80 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage  0.0020 - 0.0040 cm/cm
@Thickness 1.00 mm
0.0020 - 0.0040 in/in
@Thickness 0.0394 in
Absolute Drying
 0.0060 - 0.0080 cm/cm
@Thickness 3.00 mm
0.0060 - 0.0080 in/in
@Thickness 0.118 in
Absolute Drying
Melt Flow 5.0 g/10 min5.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121Absolute Drying; ASTM-D785
Tensile Strength, Ultimate  100 MPa
@Temperature 80.0 °C
14500 psi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 112 MPa
@Temperature 80.0 °C
16200 psi
@Temperature 176 °F
Absolute Drying; ASTM-D638
 165 MPa
@Temperature 23.0 °C
23900 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 220 MPa
@Temperature 23.0 °C
31900 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D638
 245 MPa
@Temperature -40.0 °C
35500 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 270 MPa
@Temperature -40.0 °C
39200 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Elongation at Break 2.0 %2.0 %Absolute Drying; ASTM-D638
 2.2 %2.2 %Practical Use (Water Absorption 0.8%); ASTM-D638
Flexural Strength  155 MPa
@Temperature 80.0 °C
22500 psi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 175 MPa
@Temperature 80.0 °C
25400 psi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 260 MPa
@Temperature 23.0 °C
37700 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 330 MPa
@Temperature -40.0 °C
47900 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 345 MPa
@Temperature 23.0 °C
50000 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 360 MPa
@Temperature -40.0 °C
52200 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Flexural Modulus  5.90 GPa
@Temperature 80.0 °C
856 ksi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 7.00 GPa
@Temperature 80.0 °C
1020 ksi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 12.5 GPa
@Temperature 23.0 °C
1810 ksi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 15.0 GPa
@Temperature 23.0 °C
2180 ksi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 15.1 GPa
@Temperature -40.0 °C
2190 ksi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 16.0 GPa
@Temperature -40.0 °C
2320 ksi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Compressive Strength 180 MPa26100 psiAbsolute Drying; ASTM-D695
Izod Impact, Notched  1.40 J/cm
@Temperature -40.0 °C
2.62 ft-lb/in
@Temperature -40.0 °F
Absolute Drying; ASTM-D256
 1.50 J/cm
@Temperature -40.0 °C
2.81 ft-lb/in
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
 1.70 J/cm
@Temperature 23.0 °C
3.18 ft-lb/in
@Temperature 73.4 °F
Absolute Drying; ASTM-D256
 1.90 J/cm
@Temperature 23.0 °C
3.56 ft-lb/in
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmPractical Use (Water Absorption 0.8%); ASTM-D257
 1.00e+12 ohm-cm1.00e+12 ohm-cmAbsolute Drying; ASTM-D257
Dielectric Strength  20.0 kV/mm
@Thickness 2.00 mm
508 kV/in
@Thickness 0.0787 in
Practical Use (Water Absorption 0.8%); ASTM-D149
 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Arc Resistance 33 sec33 secPractical Use (Water Absorption 0.8%); ASTM-D495
 40 sec40 secAbsolute Drying; ASTM-D495
Comparative Tracking Index 550 V550 VIEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C10.0 µin/in-°FAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 243 °C469 °FAbsolute Drying; ASTM-D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 120 - 140 °C248 - 284 °F
Injection Pressure 40.0 - 80.0 MPa5800 - 11600 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo GLAMIDE® T-402FR Nylon-6
Toyobo GLAMIDE® T-521 Nylon-6
Toyobo GLAMIDE® T-808-02 Nylon-6
Toyobo GLAMIDE® TY-835TC Nylon-66
Toyobo GLAMIDE® T-422VOR Nylon-6

PTOY936 / 107487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.