MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 5712 Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).

Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is lightly dusted with talc. Higher heat resistance, tensile and bond strengths can be achieved with the addition of diisocyanates, peroxides, epoxies, and polyfunctional amides.

Available in Americas, Europe, Middle East, Africa, India and Asia

Uses: Solution and melt coating.

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Viscosity 223000 cP
@Temperature 204 °C
Melt Viscosity; ASTM D1084-88
Brookfield Viscosity 3000 cP
@Temperature 23.0 °C
20% T.S. in MEK; 20 RPM; RVT Spindle #2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ASTM D2240
Tensile Strength, Ultimate 37.2 MPaASTM D412
Tensile Strength, Yield 5.90 MPa100% elongation; ASTM D412
 9.00 MPa300% elongation; ASTM D412
Elongation at Break 600 %ASTM D412
Peel Strength 1.40 kN/mT-Peel, Aluminum Foil; ASTM D1876-72
 6.50 kN/mT-Peel, Mylar Foil; ASTM D1876-72
 8.10 kN/mFinal
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -39.0 °CDSC
Ring & Ball Softening Point 184 °CASTM E-28-92
 
Descriptive Properties
Gradient Bar Tack Temperature (°C)124
Green Strength (kN/m)6.5
Heat Activation (°C)54
Heat Resistance (°C)70Lubrizol 899
Open Tack Time (hour)2
Open Time (sec)225ASTM D4497-94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane

PNOVEON551 / 121442

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.