MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zeus Absorv® Poly(L-lactide) (PLLA) Bioabsorbable Polymer
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: Absorv® Bioabsorbable products are particularly suitable for medical applications seeking to provide an alternative to metal stents or other components. Absorv® products are extruded from synthetic homopolymers such as PLA, PGA, PCL, and others. These materials can be combined by Zeus' design engineers as copolymers to achieve controlled degradation profiles for absorbable scaffolds. Zeus' extruded products can be precision laser cut or coated with medications to create drug-eluting implants.

Applications include:

  • Orthopedic – fracture fixation plates, pins and screws, bone augmentation, nails (scaffolding)
  • Dental – packing, dry socket treatment, scaffolding
  • Surgical – ligament repair, wound closure (sutures, suture anchors, skin staples, and adhesives), adhesion barriers, drug delivery, antineoplastic delivery, ligating clips, hemostasis clips, temporary RO markers
  • Stents – vascular, coronary, biliary, ureteral, esophageal, etc.
  • Tissue engineering – 3-D structures, electrospinning, molded, extruded vascular graft with scaffolding, bowel anastomosis and ureteral anastomosis, guided nerve regeneration, percutaneous devices with limited in-growth, tissue engineering scaffolds, vehicles for controlled drug and therapeutic agent delivery

Key Properties:

  • Controlled/gradual rates of bioabsorption or degradation
  • Capable of safely existing in and being absorbed by the body
  • Varying strengths and stiffness
  • Absence of stress shielding associated with long term permanent implants
  • FDA-approved for medical devices
Zeus Capabilities:
  • Extruded Tubing, Profiles, Monofilament, Drawn Fiber, and Ribbon
  • 100 µm wall thicknesses available
  • Ability to compound and synthesize bioabsorbable resins for in vitro testing
  • Advanced processing and development expertise
  • Custom extrusion and processing of proprietary resins
  • Network of partners to laser cut end devices

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 65.0 MPa
Modulus of Elasticity 3.00 - 4.00 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 180 - 190 °C
Glass Transition Temp, Tg 60.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Total Mass Lost18 - 36 MonthsApproximate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Poly-L-lactide (PLLA)
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Polylactic Acid (PLA) Biopolymer
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Overview of materials for Polypropylene, Molded

PZEUS970 / 190967

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.