MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, seafood and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures

Data provided by the manufacturer, DuPont Packaging.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 400 %ASTM D882
Secant Modulus, MD 0.240 GPaASTM D882
Secant Modulus, TD 0.0450 GPaASTM D882
Impact 220Spencer Impact in J/cm; ASTM D3420
Elmendorf Tear Strength, MD 2.90 g/micron
Elmendorf Tear Strength, TD 3.30 g/micron
Dart Drop 7.10 g/micronASTM D1709B
Seal Strength <= 2600 g/25 mmVaries with seal bar temp.
Hot Tack Strength <= 2200 g/25 mmVaries with seal bar temp.; Packforsk Method
Film Tensile Strength at Break, MD 37.0 MPaASTM D882
Film Tensile Strength at Break, TD 36.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 95.0 °CDSC; ASTM D3418
Vicat Softening Point 65.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D1003
Gloss 20 %20°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 177 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1702 Zinc Ionomer Resin for Extrusion Coating

PDU615 / 33092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.