MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183-A
Linear Mold Shrinkage, Flow 0.0036 - 0.0108 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 29000 psiISO 527
Elongation at Break 3.4 %ISO 527
Tensile Modulus 1.48e+6 psiISO 527
Flexural Strength 42100 psiISO 178
Flexural Modulus 1.38e+6 psiISO 178
Izod Impact, Notched (ISO) 6.19 ft-lb/in²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 500 °F
Deflection Temperature at 1.8 MPa (264 psi) 482 °FISO 75-2
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 500 - 518 °F
Middle Barrel Temperature 518 - 536 °FCompression Zone
Front Barrel Temperature 536 - 554 °F
Nozzle Temperature 520 - 535 °F
Melt Temperature 518 - 572 °F
Mold Temperature 176 - 248 °FSurface
Drying Temperature 176 °FDehumidifying Dryer
Dry Time 3 - 4 hour
Moisture Content <= 0.20 %
Back Pressure 20.0 - 50.0 psi
Fill Speed 200 - 300 mm/secPeripheral Screw Speed
 
Descriptive Properties
Injection Speed (cm3/sec)120 - 170 cm3/sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A 205F Nylon 66, EH50
BASF Ultradur® B 2550 PBT
Domo TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0

PRHO03n / 65934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.