MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Amco PRIMATOP PP HOMO 038X Fiber Grade Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: PP HOMO 038X features low water carryover. Applications include woven fabric and bags, rope and cordage, woven carpet backing, and woven geotextile fabrics.

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Index of Compound 3.8 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97ASTM D785
Hardness, Shore D 71ASTM D2240
Tensile Strength, Yield 5350 psi50 mm/min; ASTM D638
Flexural Modulus 230 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.700 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 214 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
Amco PRIMATOP PP HOMO 200NA Homopolymer Polypropylene

PATOP019 / 79962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.