MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain bikes.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Water Absorption 7.7 - 8.3 %7.7 - 8.3 %ISO 62
Moisture Absorption at Equilibrium 2.3 - 2.9 %2.3 - 2.9 %ISO 62
 2.6 %2.6 %50% RH
 8.0 %8.0 %Saturation
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/in
Melt Flow 55.8 g/10 min55.8 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 181 MPa26300 psiISO 2039-1
Tensile Strength at Break  126 MPa
@Temperature 23.0 °C
18300 psi
@Temperature 73.4 °F
ISO 527-1/-2
 156 MPa
@Temperature -40.0 °C
22600 psi
@Temperature -40.0 °F
ISO 527-1/-2
Elongation at Break 2.9 %2.9 %ISO 527-1/-2
Modulus of Elasticity 6.10 GPa885 ksiISO 527-1/-2
Flexural Strength 189 MPa27400 psiISO 178
Flexural Modulus 6.10 GPa885 ksiISO 527
Charpy Impact Unnotched 4.70 J/cm²
@Temperature 23.0 °C
22.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.590 J/cm²
@Temperature 23.0 °C
2.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 214 °C417 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 187 °C369 °FISO 75-1/-2
Decomposition Temperature >= 300 °C>= 572 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 260 °C500 °FFeed Zone
Zone 2 370 °C698 °FCompression
Zone 3 280 °C536 °FMetering-zone
Zone 4 280 °C536 °FNozzle
Melt Temperature 270 - 290 °C518 - 554 °FInjection Molding/Extrusion
 280 °C536 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection Molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
Commercial StatusEurope and North America
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry)
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned)

PBASG0379 / 132012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.