MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: TECHNYLSTAR™ AFX 218 V50 is based on a patented high flow polyamide 66 resin, heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is available in black and natural colors.

Benefits: Due to its outstanding flow characteristics, the product shows exceptional processing behavior and excellent surface aspect of the finished part.

Available in: Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: The product is particularly suitable for all applications where a high rigidity is required: typically structural parts or brackets for the automotive industry. Its high mechanical performance allows that product to be an alternative to metal parts.

Product data for dry samples.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccISO 1183/A
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cm
Linear Mold Shrinkage, Transverse 0.0042 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 255 MPaISO 527 Type 1A
Tensile Stress at Strain 100 MPa
@Strain 1 %
 145 MPa
@Strain 2 %
 180 MPa
@Strain 3 %
Elongation at Break 2.5 %ISO 527 Type 1A
Tensile Modulus 17000 MPaISO 527 Type 1A
Flexural Strength 380 MPaISO 178
Flexural Modulus 15000 MPaISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) 88.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 100 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 264 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 256 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
1210
Glow Wire Ignition Temperature 675 °C
@Thickness 0.800 mm
ISO 60695-2-12
Glow Wire Flammability Index 650 °C
@Thickness 0.800 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 270 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Celanese VECTRA E115i LCP, 15% Glass Reinforced
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry)
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled

PRHOD819 / 138050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.