MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UBE Tyranno Grade SA Ceramic High Temperature Fiber
Categories: Ceramic; Other Engineering Material; Composite Fibers

Material Notes: Tyranno SA Fiber is the continuous ceramic fiber consisting of Si, Ti, C and O. Advanced composites reinforced by the Tyranno Fiber are used in the environmental preservation field in the future such as ultra high speed transportation, energy savings, CO2 and NOx reduction, and purification of the exhaust fumes. The reinforcing fibers need to meet the demand for these applications such as high temperature stability, high strength, and high reliability in the extreme environment. Tyranno Fiber SA is a polycrystalline SiC fiber containing small amount of Aluminum, produced by decomposing and subsequently sintering of the amorphous Si-Al-C-O fiber. Tyranno Fiber SA is very stable fiber------for example, the weight loss of this fiber was only 1.8wt% at 2200°C. The initial strength of this fiber was perfectly maintained up to 1900°C in Argon. In spite of its crystalline structure, as the diameter is very small (~10µm), Tyranno Fiber SA is flexible enough to weave to fabrics. Its excellent creep resistance at high temperature has been already confirmed.

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/cc
Filament Diameter 10 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2400 MPa
Elongation at Break 0.70 %
Tensile Modulus 380 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.669 J/g-°C
Thermal Conductivity 65.0 W/m-K
Maximum Service Temperature, Inert 1900 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 2.0 %
Carbon, C 31 %
Oxygen, O <= 1.0 %
Silicon, Si 67 %
 
Descriptive Properties
Number of Filaments800-1600 fil./yarn
Structurecrystalline
Tex180-190 g/1000m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber
UBE Tyranno Grade ZMI Ceramic High Temperature Fiber
Specialty Materials SCS-6 Silicon Carbide Monofilament
3M Nextel™ 650 Composite Ceramic Fiber
3M Nextel™ 610 Composite Ceramic Fiber

CUBE251 / 2732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.