MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel CREUSABRO® 4800 Advanced Technology in Wear Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: CREUSABRO® 4800(P) is a wear resistant steel offering up to 50% extra in service life compared with a 400 HB water quenched steel. CREUSABRO® 4800(P) combines several modern metallurgical concepts which, depending on thickness, use different combinations of an enriched chemical analysis (Cr, Mo, Ti…) and controlled quenching rate. Creusabro® 4800(P) is designed to provide the optimum combination of wear resistance controlled hardness and ease of processing. Rather then using just a high hardness level, it achieves this aim by using proven and controlled metallurgical mechanisms, which are more complex but more efficient then the simple effect of hardness alone.
  • Work-hardening and Cr Mo micro-carbides, the basic CREUSABRO® concept
  • TRIP (TRansformation Induced by Plasticity) effect originally developed with CREUSABRO® 8000
  • Reinforcement of the structure with Titanium carbides.
The limited as delivered hardness of Creusabro® 4800(P) makes processing operations like cutting, machining and forming no more difficult then processing 400HB water quenched steel. Creusabro® 4800(P) is ideal for applications in mines and quarries, cement and the Steelmaking industries, publics works and agricultural machinery. It is suitable for all types of abrasion, sliding or impact, dry or wet media including high temperature abrasion up to 350°C.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 340 - 400340 - 400Typical
Tensile Strength, Ultimate 1200 MPa174000 psiTypical
Tensile Strength, Yield 900 MPa131000 psiTypical
Elongation at Break 12 %12 %Typical
Modulus of Elasticity 205 GPa29700 ksiTypical
Charpy Impact 45.0 J
@Temperature -20.0 °C
33.2 ft-lb
@Temperature -4.00 °F
Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.4 µm/m-°C
@Temperature 20.0 - 100 °C
6.89 µin/in-°F
@Temperature 68.0 - 212 °F
 13.1 µm/m-°C
@Temperature 20.0 - 200 °C
7.28 µin/in-°F
@Temperature 68.0 - 392 °F
 13.9 µm/m-°C
@Temperature 20.0 - 300 °C
7.72 µin/in-°F
@Temperature 68.0 - 572 °F
 14.7 µm/m-°C
@Temperature 20.0 - 500 °C
8.17 µin/in-°F
@Temperature 68.0 - 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.20 %<= 0.20 %
Chromium, Cr <= 1.9 %<= 1.9 %
Iron, Fe 95.477 - 99.8 %95.477 - 99.8 %As remainder
Manganese, Mn <= 1.6 %<= 1.6 %
Molybdenum, Mo <= 0.40 %<= 0.40 %
Nickel, Ni 0.20 %0.20 %
Phosphorus, P <= 0.018 %<= 0.018 %
Sulfur, S <= 0.0050 %<= 0.0050 %
Titanium, Ti <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel
Industeel CREUSABRO® 4000 High Wear Resistant Steel
AISI 1035 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper
Industeel SUPERELSO® 690CR Quenched and Tempered High Strength Steel for Leg Components of Jack-up Rigs
AISI 4140H Steel, oil quenched, tempered 540°C (1000°F), 25 mm (1 in.) round

NINDUST56 / 17594

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.