MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFINE™ PP Polypropylene (PP)
Categories: Polymer; Thermoplastic; Polyolefin; Polypropylene (PP); Polypropylene Copolymer

Material Notes: TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical properties than other typical polyolefin materials, it is light weight, weldable, and unaffected by moisture. Ensinger's processing technology provides quality in TECAFINE™ PP stock shapes.

  • Excellent chemical resistance (TECAFINE™ PP is resistant to organic chemicals, solvents, mineral acids, and inorganic salts)
  • Weldable
  • High purity (nonparticulating and suitable for high purity environments)
  • FDA compliant (meets FDA 21 DFR 177.1520)
  • Light wieght (has a specific gravity of less than 1)
  • Moisture resistant (unaffected by water or moist environments)
  • Great quality (Ensinger's extrusion expertise means users consistently obtain the highest quality polypropylene stock shapes)

TECAFINE™ PP's excellent chemical resistance and high purity characteristics make it ideal for use in the food-processing and chemical-processing industries. Common applications include pump and valve components, tanks, laboratory equipment, and other parts in contact with corrosive environments.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc0.0330 lb/in³ASTM D792
Water Absorption 0.010 - 0.030 %
@Temperature 22.8 °C,
Time 86400 sec
0.010 - 0.030 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength at Break 32.4 MPa
@Temperature 22.8 °C
4700 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 100 %
@Temperature 22.8 °C
100 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 0.896 GPa
@Temperature 22.8 °C
130 ksi
@Temperature 73.0 °F
ASTM D638
Flexural Strength 41.4 - 55.2 MPa
@Temperature 22.8 °C
6000 - 8000 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 1.24 GPa
@Temperature 22.8 °C
180 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.481 J/cm
@Temperature 22.8 °C
0.900 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm
@Temperature 22.8 °C
1.00e+17 ohm-cm
@Temperature 73.0 °F
ASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz,
Temperature 22.8 °C
2.2
@Frequency 60 Hz,
Temperature 73.0 °F
50% RH; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Melting Point 166 °C330 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FASTM D648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene Copolymer
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin
BASF Procom® GC30H 251 Polypropylene
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade

PENSIN020 / 92837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.