MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 105F BK010 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced, UV Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Water Absorption 0.95 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
 8.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 2.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/gSulfuric acid 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.013 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50% RH; ISO 527-1/-2
 85.0 MPaDAM; ISO 527-1/-2
Elongation at Break 24 %Nominal; DAM; ISO 527-1/-2
 >= 50 %Nominal; 50% RH; ISO 527-1/-2
Elongation at Yield 4.3 %DAM; ISO 527-1/-2
 25 %50% RH; ISO 527-1/-2
Tensile Modulus 1500 MPa50% RH; ISO 527-1/-2
 3200 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.37DAM
 0.4350% RH
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 55.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 55.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 1340 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 600 MPa1000h; 50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 263 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CDAM; ISO 75-1/-2
Vicat Softening Point 240 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 40.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 V-2
@Thickness 0.710 mm
DAM; IEC 60695-11-10
 V-2
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Oxygen Index 27 %DAM; ISO 4589-1/-2
Glow Wire Test 700 °C
@Thickness 0.750 mm
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.00 mm
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.50 mm
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 2.00 mm
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 3.00 mm
No Flame; DAM; IEC 60335-1
Glow Wire Ignition Temperature 725 °C
@Thickness 0.750 mm
DAM; IEC 60695-2-13
 725 °C
@Thickness 1.00 mm
DAM; IEC 60695-2-13
 725 °C
@Thickness 1.50 mm
DAM; IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
DAM; IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 70.0 °COptimum, Injection
 50.0 - 90.0 °CInjection
Ejection Temperature 190 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)6.6VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66,,M1CG1L1R,S14-030
Max. screw tangential speed (m/s)0.4Injection
Odor Class2.5VDA 270
Part Marking Code>PA66<ISO 11469
PolymerPA66
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® T835FRUV NC010 PBT
Celanese Zytel® 103FHSA NC010 PA66
RTP Company RTP 200 D UV Nylon 6/12 (PA); UV Stabilized
Celanese Zytel® 45HSB NC010 PA66
Celanese Zytel® 70G13HS1L BK031 PA66-GF13

PDSX5304 / 197944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.