MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.

Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.

EVAL™ is now produced as a part of the Kuraray product line.

Key Words: Ethylene Vinylalcohol
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium 3.9 %65% RH
 3.9 %65% RH
 8.5 %100% RH
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm40°C, 90% RH
Oxygen Transmission 0.00800 cc-mm/m²-24hr-atm20°C; 65% RH; Permeability increases significantly at higher moisture content.
Thickness 0.600 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 180 %10%/min.; ASTM D638
Film Elongation at Break, TD 140 %10%/min.; ASTM D638
Secant Modulus, MD 2.00 GPaYoungs Modulus, ASTM D638, 10%/min.
Secant Modulus, TD 1.90 GPaYoungs Modulus, ASTM D638, 10%/min.
Elmendorf Tear Strength MD 380 gASTM D638
Elmendorf Tear Strength TD 300 gASTM D638
Elmendorf Tear Strength, MD 633 g/mil0.6 mil; ASTM D638
Elmendorf Tear Strength, TD 500 g/mil0.6 mil; ASTM D638
Film Tensile Strength at Break, MD 80.0 MPa10%/min.; ASTM D638
Film Tensile Strength at Break, TD 52.0 MPa10%/min.; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 4.70e+12 ohm-cm
Surface Resistance 1.90e+15 ohm
Dielectric Constant 5.5Frequency Not Specified
Dissipation Factor 0.21Frequency Not Specified
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
Estimated by MatWeb from similar grades
 110 µm/m-°C
@Temperature 100 °C
Estimated by MatWeb from similar grades
Specific Heat Capacity 2.40 J/g-°CEstimated by MatWeb from similar grades
Thermal Conductivity 0.340 W/m-KFor EVAL F101
Melting Point 181 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 1.5 %65% RH
Gloss 90 %65% RH

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui ADMER® NF468A PE Type Polyolefin

PEVALD / 37303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.