MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Visico™/Visico™ LE4423/LE4438 Polyethylene Compound, Crosslinkable
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Visico™ LE4423 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4423 and Visico™ LE4438 is a combination of a Visico™ base material and a catalyst master batch which accelerates the moisture-induced crosslinking reaction. When properly mixed, addition of 5 parts of Visico™ LE4438 to 95 parts of Visico™ LE4423, insulation with excellent thermo-oxidative stability, also in contact with copper as well as aluminum, is achieved. Applications: Insulation of low voltage cables for the range up to 6 kV. Additives: Visico™ LE4423 / Visico™ LE4438 contains antioxidant and metal deactivator. Visico™ LE4423 contains a permanent scorch retardant additive, ensuring safe processing and enabling the use of a highly active crosslinking catalyst. Specifications: Visico™ LE4423 / Visico™ LE4438 in combination meets these applicable requirements when processed using sound extrusion and testing procedure: ASTM D 1248 Type I, Class A, Category 4; IEC 60502-1; HD 603 S1; HD 604 S1; NEMA WC 70; and NEMA WC 71.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccmixture 95:5; ISO 1183/ISO 1872-2
ESCR 10% Igepal® >= 96 hour
@Temperature 50.0 °C
F20; IEC 60811-4-1/B
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 521s; ISO 868
Tensile Strength at Break <= 11.25 MPaafter aging (240h, 135°C); IEC 60811-1-2
 >= 15.0 MPa250mm/min; ISO 527
Elongation at Break >= 300 %250mm/min; ISO 527
Tensile Set 0.00 %
@Temperature 200 °C
Permanent Deformation at 0.2 MPa after 60% elongation under load; IEC 60811-2-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+6 ohm-cmIEC 60093
Dielectric Constant 2.3
@Frequency 50000 Hz
IEC 60250
Dielectric Strength >= 22.0 kV/mmIEC 60243
Dissipation Factor 0.00050
@Frequency 50000 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Zone 1 150 °C
Zone 2 170 °C
Zone 3 170 °C
Zone 4 170 °C
Die Temperature 170 °C
Shelf Life 18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Borealis SuperCOPO™ LE4205R Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE0592S Polyethylene

PBOREA604 / 108863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.