MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alclad Aluminum 2014-T3
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Used in applications requiring high strength/hardness, including elevated temperature uses. Specific applications include heavy duty forgings, plate, and extrusions for aerospace fittings, wheels, tanks, and major structural components, heavy duty automotive frame and suspension componentry. 2014 exhibits poor corrosion resistance for an aluminum alloy so the clad version is used when necessary.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes: Composition for AA 2014 (not Alclad 2014 specifically).
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A82014; Alclad 2014-T3; Alclad 2014-T3; Al2014-T3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³For AA2014 (Not Alclad)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 434 MPa63000 psiAA; Typical
 >= 370 MPa
@Thickness 0.508 - 0.610 mm
>= 53700 psi
@Thickness 0.0200 - 0.0240 in
Flat sheet
 >= 380 MPa
@Thickness 0.635 - 0.991 mm
>= 55100 psi
@Thickness 0.0250 - 0.0390 in
Flat sheet
 >= 395 MPa
@Thickness 1.02 - 6.32 mm
>= 57300 psi
@Thickness 0.0400 - 0.249 in
Flat sheet
Tensile Strength, Yield 276 MPa40000 psiAA; Typical
 >= 230 MPa
@Thickness 0.508 - 0.610 mm
>= 33400 psi
@Thickness 0.0200 - 0.0240 in
Flat sheet
 >= 235 MPa
@Thickness 0.635 - 0.991 mm
>= 34100 psi
@Thickness 0.0250 - 0.0390 in
Flat sheet
 >= 240 MPa
@Thickness 1.02 - 6.32 mm
>= 34800 psi
@Thickness 0.0400 - 0.249 in
Flat sheet
Elongation at Break  14 %
@Thickness 0.508 - 0.610 mm
14 %
@Thickness 0.0200 - 0.0240 in
Flat sheet
 14 %
@Thickness 0.635 - 0.991 mm
14 %
@Thickness 0.0250 - 0.0390 in
Flat sheet
 15 %
@Thickness 1.02 - 6.32 mm
15 %
@Thickness 0.0400 - 0.249 in
Flat sheet
 20 %
@Thickness 1.59 mm
20 %
@Thickness 0.0625 in
AA; Typical
Modulus of Elasticity 72.4 GPa10500 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Shear Strength 255 MPa37000 psiAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 502 °C935 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.4 - 95 %90.4 - 95 %As remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 3.9 - 5.0 %3.9 - 5.0 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.20 - 0.80 %0.20 - 0.80 %
Manganese, Mn 0.40 - 1.2 %0.40 - 1.2 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 0.50 - 1.2 %0.50 - 1.2 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alclad Aluminum 2014-O
Aluminum 2014-T4; 2014-T451
Alclad Aluminum 2014-T6, T651
Aluminum 2014-T3
Aluminum 2011-T3

MA2014AT3 / 8842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.