MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded; Acrylic, Optical Grade, Molded

Material Notes: Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists gamma ray radiation sterilization which also meet US Pharmacopoeia XXI class VI toxicity requirements, and FDA food additive regulation 21 CFR 177.1010 (acrylic and modified acrylic plastics, semi-rigid, and rigid).

Information provided by Plaskolite West, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D-955
Melt Flow 3.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8000 psiASTM D-638
Elongation at Break 25 %ASTM D-638
Modulus of Elasticity 290 ksiASTM D-638
Flexural Strength 12.0 ksiASTM D-790
Izod Impact, Notched 0.800 ft-lb/in
@Thickness 6.35 mm
ASTM D-256
Gardner Impact 25.0 in-lb
@Thickness 3.17 mm
Falling Weight; ASTM D-3029 GB
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CASTM D-696
Maximum Service Temperature, Air 50.0 °CUL-746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 180 °FASTM D-648
Vicat Softening Point 220 °FASTM D-1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %ASTM D-1003
Transmission, Visible 92 %ASTM D-1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin
Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin
Trinseo Solarkote™ PB Acrylic

PCONT046 / 150603

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.