MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Cures to a low Shore A hardness
  • Excellent optical clarity
  • Easy to remove
  • Ideal for retrievability
  • Convenient handling
  • Room temperature curing
Product Description: Master Bond Super Gel 9 is a two component, urethane modified epoxy system that cures readily at room temperature to form a soft, resilient, gel-like system with good dimensional stability. Its hardness is exceptionally low, about 5-10 Shore A. One can accomplish retrievability with a sharp knife or razor blade and Super Gel 9 will not shatter. It has a very convenient two to one mix ratio by weight or volume, along with an extremely low viscosity and exotherm enabling it to be cast in larger sections up to 2-3 inches thick. Super Gel 9 has wonderful optical clarity. The combination of its easy handling and cured properties enables this versatile system to be used in a variety of applications, especially the encapsulation of sensitive electronic parts and sealing delicate optical components. It can also be used in acoustical applications where dampening properties may be desirable. This exceptional softness allows it to be easily repairable and confers it with unsurpassed thermal cycling and mechanical shock resistance. Super Gel 9 bonds well to an array of substrates, such as metals, glass, ceramics and many rubbers and plastics. It has a remarkably long working life of 7-9 hours depending on the mass that is mixed (the smaller the mass, the longer the working life). It has very good chemical resistance to water, oils and fuels. The service temperature range is -100°F to +200°F. The color of both Parts A and B are clear. This multi-functional system is widely used in the aerospace, electronic, optical, electro-optical and other specialty industries where this unique blend of properties is needed.

Product Advantages:

  • Easy handling; two to one mix ratio by weight or volume; low viscosity
  • Very low exotherm; remarkably long working life
  • Exceptionally soft and resilient
  • Good dimensional stability
  • Easily repairable; widely used for retrieving components
  • Often used in conjunction with sensitive electronic and optical components

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 75 - 150 cPPart B
 3000 - 9000 cPMixed
 7000 - 12000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A <= 5.0
Tensile Strength 400 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 4.1
@Frequency 60 Hz
Dielectric Strength >= 420 V/mil
@Thickness 3.17 mm
Dissipation Factor 0.090
@Temperature 15.6 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -100 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5253
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 8.00 hour24-48 hours at 75°F, plus 140-150°F
 96.0 - 168 hour
@Temperature 23.9 °C
Working Life 360 - 480 minAfter mixing, 200 gram batch
 420 - 540 minAfter mixing, 100 gram batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio2:1 by weightPart A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond Super Gel 9AO Thermally Conductive Urethane Modified Epoxy Gel
Master Bond FL901AO One Component Thermally Conductive Epoxy Adhesive Film
Master Bond FL901S One Component, Silver Filled Epoxy

PMASTM967 / 185560

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.