MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik BREAK-THRU® S 233 Surfactants
Categories: Fluid

Material Notes: BREAK-THRU® S 233 is a patented non-ionic trisiloxane surfactant.

Application: In contrast to other surfactants of this class, BREAK-THRU® S 233 does not show super spreading, yet, exhibits excellent wetting through normal spreading. However, it does dramatically reduce surface tension of spray solutions to about 23 mN/m. It increases the deposition of actives better than other trisiloxanes and it improves significantly the penetration of actives into plant tissue. It is specifically suited for enhancing the bio-logical performance of systemic and semi-systemic products not only for herbicides, also for fungicides, insecticides and plant growth regulators. BREAK-THRU® S 233 can be used in tank mix applications without any incompatibility problems. It can as well be used in formulations e. g. EC, SC, SL. For tank-mixtures, pesticides manufacturers may suggest a rate of a non-ionic surfactant to be used with their product. Follow the corresponding label recommendation. However, if the crop protection label does not have a specific recommendation for adjuvant use, BREAK-THRU® S 233 should be applied at rates listed here. Further experimental work may be required to identify the specific dose rate of BREAK-THRU® S 233 when it is incorporated into a formulation with a crop protection product. Careful observation of spray performance in a trial application with the tank-mixture to be sprayed is advised to determine proper and efficient surfactant rates.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 - 1.03 g/cc
Viscosity 60 - 140 cP
 
Thermal PropertiesOriginal ValueComments
Pour Point 5.00 °C
Flash Point >= 65.0 °C
 
Descriptive Properties
AppearanceColorless to pale straw liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® S 200 Surfactants
Evonik BREAK-THRU® DA 646 Surfactants

PEVONIL706 / 196910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.