MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tritan™ Renew LX101-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan™ Renew LX101-50 is an amorphous copolyester with excellent appearance and clarity. Tritan Renew LX101-50 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan Renew LX101-50 was developed for the cosmetic, fragrance, and personal care markets. Tritan Renew LX101-50 can easily be converted into articles for application in Consumer and Personal Care markets by injection molding, extrusion blow molding, and injection blow molding. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. .

Applications

  • Bottles-color cosmetics pkg
  • Bottles-fragrance pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Ease of processing
  • Excellent clarity
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Outstanding impact resistance
  • Quick cycle times

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 cm/cm0.00500 - 0.00700 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D785
Tensile Strength at Break 53.0 MPa7690 psiASTM D638
Tensile Strength, Yield 43.0 MPa6240 psiASTM D638
Elongation at Break 210 %210 %ASTM D638
Elongation at Yield 6.00 %6.00 %ASTM D638
Tensile Modulus 1.55 GPa225 ksiASTM D638
Flexural Yield Strength 62.0 MPa8990 psiASTM D790
Flexural Modulus 1.55 GPa225 ksiASTM D790
Izod Impact, Notched  1.10 J/cm
@Temperature -40.0 °C
2.06 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 9.80 J/cm
@Temperature 23.0 °C
18.4 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy  61.0 J
@Temperature 23.0 °C
45.0 ft-lb
@Temperature 73.4 °F
@ Max. Load; ASTM D3763
 66.0 J
@Temperature -40.0 °C
48.7 ft-lb
@Temperature -40.0 °F
@ Max. Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 1.00 %<= 1.00 %ASTM D1003
Transmission, Visible 90.0 %90.0 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 282 °C500 - 540 °F
Mold Temperature 38.0 - 66.0 °C100 - 151 °F
Drying Temperature 88.0 °C190 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4211 / 323834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.