MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Stratasys® Rigur Rubber-Like PolyJet 3D Printing Polymer Combination: Primary: TANGOBLACKPLUS FLX980 / TANGOPLUS FLX930; Secondary: VEROBLACKPLUS RGD875
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Using two Polyjet printing materials, manufacturers can print prototypes that simulate the appearance and functionality of polypropylene to test form, fit, and function for applications such as snap-fit assemblies, hinges, durable housings, and packaging. Rigur (RGD450) acts as an advanced polypropylene material substitute that offers durability and great surface finishes. Use Rigur in any office-friendly environment to gain reliable performance and stable prototypes. Durus (RGD430) is the original Simulated Polypropylene material that exhibits great impact resilience and an elongation at break of 44%.

Characteristics

  • Opaque
  • Tough
  • Dimensionally stable
Options
  • Rigur is an office-friendly material engineered to deliver reliable performance and impressive, dimensionally stable prototypes.
  • Rigur comes in a bright, true white with PolyJet technology’s signature fine resolution and smooth curves.
Uses
  • Reusable containers and packaging
  • Flexible, snap-fit applications and living hinges
  • Toys, battery cases, laboratory equipment
  • Loudspeakers and automotive component
Advantages
  • Versatility
  • Fine detail
  • Superior toughness
  • Bright white color for sleek prototypes

Information provided by Proto3000

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35.0 - 40.0FLX2140-DM; FLX2040-DM; ASTM D2240
 45.0 - 50.0FLX2150-DM; FLX2050-DM; ASTM D2240
 57.0 - 63.0FLX2160-DM; FLX2060-DM; ASTM D2240
 68.0 - 72.0FLX2170-DM; FLX2070-DM; ASTM D2240
 80.0 - 85.0FLX2185-DM; FLX2085-DM; ASTM D2240
 92.0 - 95.0FLX2195-DM; FLX2095-DM; ASTM D2240
Tensile Strength 1.30 - 1.80 MPaFLX2140-DM; FLX2040-DM; ASTM D412
 1.90 - 3.00 MPaFLX2150-DM; FLX2050-DM; ASTM D412
 2.50 - 4.00 MPaFLX2160-DM; FLX2060-DM; ASTM D412
 3.50 - 5.00 MPaFLX2170-DM; FLX2070-DM; ASTM D412
 5.50 - 7.00 MPaFLX2185-DM; FLX2085-DM; ASTM D412
 8.50 - 10.0 MPaFLX2195-DM; FLX2095-DM; ASTM D412
Elongation at Break 35.0 - 45.0 %FLX2195-DM; FLX2095-DM; ASTM D412
 55.0 - 65.0 %FLX2185-DM; FLX2085-DM; ASTM D412
 65.0 - 80.0 %FLX2170-DM; FLX2070-DM; ASTM D412
 75.0 - 85.0 %FLX2160-DM; FLX2060-DM; ASTM D412
 95.0 - 110 %FLX2150-DM; FLX2050-DM; ASTM D412
 110 - 130 %FLX2140-DM; FLX2040-DM; ASTM D412
Tear Strength 5.39 - 7.35 kN/mFLX2140-DM; FLX2040-DM; ASTM D624
 7.35 - 9.32 kN/mFLX2150-DM; FLX2050-DM; ASTM D624
 10.8 - 12.7 kN/mFLX2160-DM; FLX2060-DM; ASTM D624
 15.2 - 17.2 kN/mFLX2170-DM; FLX2070-DM; ASTM D624
 22.6 - 24.5 kN/mFLX2185-DM; FLX2085-DM; ASTM D624
 40.2 - 43.1 kN/mFLX2195-DM; FLX2095-DM; ASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROTO860 / 322873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.