MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper-Nickel-Phosphorus alloy, UNS C19000, TF00 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Spot Weld, Seam Weld

Common Fabrication Processes: Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Roll Threading and Knurling; Shearing; Swaging

Typical uses: Connectors; Electronic Parts for Electron Tube Components; Electronic Parts for Power Tube Components; High Strength Electrical Conductors; Bolts; Clips; Cotter Pins; Nails; Screws

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 65.0 ksi
@Thickness 2.03 mm
Tensile Strength, Yield 40.0 ksi
@Thickness 2.03 mm
0.2% Offset
 40.0 ksi
@Thickness 2.03 mm
0.5% Ext
Elongation at Break 25 %
@Thickness 2.03 mm
Tensile Modulus 18000 ksi
Modulus of Rigidity 6800 ksi
Poissons Ratio 0.32Calculated
Machinability 30 %
Forgeability 65 %
Shear Strength 35.0 ksi
@Thickness 2.03 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000290 ohm-cm60% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 145 BTU-in/hr-ft²-°F
Melting Point 1900 - 1980 °F
Solidus 1900 °F
Liquidus 1980 °F
Annealing Point 900 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Solution Temperature 1300 - 1450 °F
Hot-Working Temperature 1300 - 1550 °F
Precipitation Temperature 850 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 97.4 - 99 %As Balance
Iron, Fe <= 0.10 %
Lead, Pb <= 0.050 %
Nickel, Ni 0.90 - 1.3 %
Phosphorus, P 0.15 - 0.35 %
Zinc, Zn <= 0.80 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC19000y3 / 292874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.