MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Ensinger TECAPEI® made from Ultem® 1000 PEI
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in color, and combine exceptional mechanical, thermal, and electrical properties. The addition of glass fiber reinforcement in the 2000 series, coupled with Ensinger's proprietary extrusion techniques, provides the TECAPEI™ with both greater tensile strength and rigidity, while also improving dimensional stability.

  • Excellent mechanical strength (exhibits high tensile strength at room temperature and retains a significant portion of this strength at elevated temperatures. Glass fibers further increase high-temperature strength)
  • Outstanding heat resistance (retains its physical properties at elevated temperatures)
  • Exceptional resistance to environmental forces (Environmental characteristics of TECAPEI™ include it's stress resistance)
  • Inherent flame resistance with low smoke evolution (Tested internally to UL 94 V-0)
  • High mechanical strength
  • High dielectric strength and stability
  • Low dissipation factor over a wide range of frequencies
  • Excellent machinability and finishing characteristics (TECAPEI™ can be easily machined with conventional metalworking tools, painted, hot stamped, printed, or metallized)
  • Resin used in natural grade are FDA, USP Class VI and NSF compliant

TECAPEI™ has many applications in medical, electronic/electrical, microwave, automotive, and aircraft industries.

Information Provided by Ensinger Inc.

Vendors: Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Water Absorption 0.25 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
Water Absorption at Saturation 1.25 %
@Temperature 22.8 °C
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 109ASTM D785
Tensile Strength at Break 15200 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 40 %
@Temperature 22.8 °C
ASTM D638
Elongation at Yield 7.0 - 8.0 %ASTM D638
Tensile Modulus 430000 psi
@Temperature 22.8 °C
ASTM D638
Flexural Strength 22000 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 480000 psi
@Temperature 22.8 °C
ASTM D790
Compressive Strength 21900 psiASTM D695
Compressive Modulus 480000 psiASTM D695
Shear Strength 15000 psiUltimate
Izod Impact, Notched 1.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cm1/16''; ASTM D257
Dielectric Constant 3.15
@Frequency 1000 Hz
50% RH; ASTM D150
Dielectric Strength 710 V/milIn Oil; ASTM D149
 830 V/milIn Air; ASTM D149
Dissipation Factor 0.0013
@Frequency 1000 Hz,
Temperature 22.8 °C
50% RH; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µin/in-°FASTM D696
Thermal Conductivity 1.50 BTU-in/hr-ft²-°FASTM D2214
Deflection Temperature at 0.46 MPa (66 psi) 410 °F1/4''; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 394 °F1/4''; ASTM D648
Vicat Softening Point 426 °FASTM D1525
Flammability, UL94 V-0
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
Quantum PEI - Ultem®
Overview of materials for Polyetheretherketone, Unreinforced
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI

PENSIN038 / 92855

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.