MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vapla Vaplatec 1000 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Sold in sheet form.

Information provided by Vapla.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccUNE-EN ISO 1183
Water Absorption <= 0.10 %UNE-EN ISO 62
Molecular Weight 5.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64UNE-EN ISO 868
Tensile Strength, Ultimate 27.0 MPaUNE-EN ISO 527
Tensile Strength, Yield 22.0 MPaUNE-EN ISO 527
Elongation at Break 290 %UNE-EN ISO 527
Tensile Modulus 915 MPa
Flexural Strength 23.0 MPaUNE-EN ISO 178
Charpy Impact Unnotched NBPendulum of 25 J; UNE-EN ISO 179-1
Charpy Impact, Notched 100 kJ/m²Partial Break; Pendulum of 25 J; UNE-EN ISO 179-1
Sand Slurry 100Wear Resistance; GUR 4120 = 100; UNE-EN ISO 306
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmUNE 21303
Surface Resistance >= 1.00e+12 ohmUNE 21303
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°CUNE 53126
Melting Point 135 °CUNE 1135-3
Maximum Service Temperature, Air 80.0 °CContinuous
Vicat Softening Point 80.0 °CB50; UNE-EN ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Westlake Plastics Lennite® GUR1020 (Type I) UHMW-PE For Medical Applications
Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE)
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene

PVAPLA991 / 197418

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.