MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hapco DI-PAK™ R-4807 Potting and Encapsulating Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Low viscosity, fast cure, high performance, potting and encapsulating compounds with excellent properties and FAST TURNOVER. Both are two part systems with 1:1 mix ratios by volume.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D-4669
Viscosity 240 cPASTM D-4878
Linear Mold Shrinkage 0.0015 - 0.0030 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84ASTM D-2240
Tensile Strength 6200 psiASTM D-638
Elongation at Break 11 %ASTM D-638
Modulus of Elasticity 340 ksiASTM D-638
Flexural Strength 8700 psiASTM D-790
Flexural Modulus 361 ksiASTM D-790
Izod Impact, Notched 0.230 ft-lb/inASTM D-256
Izod Impact, Unnotched 1.30 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+14 ohm-cmASTM D-270
Dielectric Constant 3.63
@Frequency 100000 Hz
ASTM D-150
 3.77
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 465 V/milASTM D-149
Dissipation Factor 0.22
@Frequency 100000 Hz
ASTM D-150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 70.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 min
@Thickness 3.17 mm
Demold
Gel Time 3.50 - 4.50 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)Black
Mix Ratio100:100Volume
 100:93Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO050 / 317109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.