MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion 84110 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: NSF listings are obtained on specific colors. The Cell Classification was determined using the notched Izod test with injection molded samples.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 828215 sec; ASTM D2240
Tensile Strength, Yield 51.2 MPa7430 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.77 GPa402 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 86.2 MPa12500 psiASTM D790
Flexural Modulus 2.83 GPa410 ksiASTM D790
Izod Impact, Notched  0.320 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.599 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
 3.20 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
5.99 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 5.70 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
Dart Drop Total Energy  60.9 J/cm
@Temperature 23.0 °C
0.114 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 86.3 J/cm
@Temperature 23.0 °C
0.162 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C37.8 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
@Thickness 3.18 mm
156 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact, Unspecified Rating
 
Descriptive Properties
Agency RatingsNSF 51
 NSF 61
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification14453ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFilm
 Profiles
 Sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Packaging XPL189 Amber 1505 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging XPL 293 FROST 1733 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging 2121 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid

PH0POL0236 / 144805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.