MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell DEXFLEX® 810-1 TPO  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: DEXFLEX® 810-1 is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. DEXFLEX® 810-1 was designed to exceed the requirements of US 5-mph bumper-impact regulations.

Applications: Bumper fascias, and other large components that must exhibit durable paintability in exterior body colors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccISO 1183
Linear Mold Shrinkage 0.0080 - 0.011 cm/cmas molded; ISO 294
 0.011 - 0.014 cm/cmafter bake; ISO 294
Melt Flow 9.0 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 18.0 MPa150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.790 GPa80x10x4 mm specimen, 2 mm/min; ISO 178
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ASTM E228

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Engineered Polymers Dexflex® 756-67 TPO
LyondellBasell DEXFLEX® 727 TPO
LyondellBasell DEXFLEX® 711 TPO
LyondellBasell Dexflex 810 BLK Thermoplastic Polyolefin
LyondellBasell DEXFLEX® 940 TPO

PSOLH14 / 68069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.