MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Evonik Cyrolon® AR Polycarbonate Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Continuously manufactured sheet with better impact and heat resistance than typical acrylic sheet. Offers protection against weathering. Used for windows, skylights, signs, displays, vending machine panels, machine guards, safety glazing, and bus shelters.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.15 %24 hrs, 23°C; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 65.0 MPaASTM D638
Elongation at Break 110 %ASTM D638
Tensile Modulus 2.34 GPaASTM D638
Flexural Yield Strength 122 MPaASTM D790
Flexural Modulus 2.34 GPaASTM D790
Compressive Yield Strength 76.0 MPaASTM D695
Izod Impact, Notched 9.70 J/cmASTM D256
Impact Test 68.0 J
@Thickness 3.00 mm
Instrumented dart; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
Short Time; ASTM D149
Dissipation Factor 0.00090
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.190 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 132 °CASTM D648
Vicat Softening Point 157 °CASTM D1525
Flammability, UL94 >= V-2UL 94 V-2, or better, depending on thickness
Oxygen Index 26 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59ASTM D542
Transmission, Visible 87 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 210 °Cforming temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NUDEC® PC Polycarbonate Sheet
Spartech UltraTuf SG Polycarbonate Sheet
Eastman Saflex® 1" (25 mm) Laminated Insulating Units (Monolithic Glass - Air Space - Laminated Glass (inboard)
Eastman Saflex® 5/16" (22 mm) Laminated Insulating Units (Monolithic Glass - Air Space - Laminated Glass (inboard)
M Chemical GUARD DOG™ UVP Benzotriazole UV Absorber

PCYR37 / 29176

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.