MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene™ Ultra UL 7710 Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 7710 is a very high flow, 26.7% wt vinyl acetate copolymer that has very good comparability with hydrocarbons tackifers and most waxes.  It is suitable for making hot melt adhesives, sealants, and wax blends.  UL 7710E contains an additive package to improve pellet flowability and handling. 

Availability:  North America, Latin America.  Additives: antiblock: no; slip: no;  thermal stabilizer: yes.  Applications: adhesives and sealants, industrial sealants, hot melt adhesives, wax blends. Forms: pellets.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D1505
Vinyl Acetate Content 26.7 %ExxonMobil Method
Melt Flow 420 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
@Time 15.0 sec
ASTM D2240
Hardness, Shore D 17
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 260 psiASTM D638
Elongation at Break 330 %ASTM D638
Flexural Modulus, 1% Secant 2200 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 149 °FPeak; ExxonMobil Method
Vicat Softening Point 117 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98940 / 238321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.