MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.

Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccASTM D792
ESCR 100% Igepal® >= 5000 hourF20, Condition C, ASTM D1693
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength, Yield 22.5 MPaASTM D638
Elongation at Break 850 %ASTM D638
Flexural Modulus 0.850 GPaSecant; ASTM D3350
Izod Impact, Notched 3.70 J/cmNotched/Unnotched not specified; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 128 °CASTM D3417
Vicat Softening Point 124 °CASTM D1525
Brittleness Temperature <= -100 °CASTM D696
Decomposition Temperature 260 °CThermal Stability; ASTM D3350
 
Processing PropertiesOriginal ValueComments
Melt Temperature 195 - 225 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin
NOVA Chemicals Novapol® HB-W952-A HDPE Extrusion Resin

PEHN2Q / 35611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.