MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Eastman Saflex® Light Bronze 0.38 mm Colored Protective Interlayer PVB Film for Glass Laminates
Categories: Polymer; Film

Material Notes: When laminated between two sheets of glass, Vanceva interlayers enhance the safety and UV protection in architectural glazing. Now available in an array of natural earth tones, these polyvinyl butyral (PVB) films also bring greater aesthetics, warmth, and serenity to any architectural space.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 5.74 W/m-K39.8 BTU-in/hr-ft²-°F
 
Descriptive Properties
Light to solar gain (LSG)0.85
Relative heat gain (RHG) W/m2515
Shading coefficient0.75
Solar absorption0.42
Solar Heat Gain Coefficient0.66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 175 Phenolic Resin
Overview of materials for PVC, Molded
Overview of materials for PVC, Extruded
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound
Eastman Saflex® Light Neutral Brown 0.38 mm Colored Protective Interlayer PVB Film for Glass Laminates

PEATM5035 / 222229

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.