MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes:

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength, Ultimate 38.0 MPa5510 psiASTM D412
Tensile Strength, Yield 4.80 MPa696 psi50% Elongation; ASTM D412
Elongation at Break 500 %500 %ASTM D412
Flexural Modulus 0.0270 GPa3.92 ksiASTM D790
Resilience 4545% Bayshore Resilience; ASTM D2632
Tear Strength 90.0 kN/m514 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3030H-18 Wheel, 1000 g load, ASTM D3489
Compression Set 16 %16 %22 hours at RT (Postcured); ASTM D395-B
 40 %
@Temperature 70.0 °C
40 %
@Temperature 158 °F
22 hours (Postcured); ASTM D395-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °FRate A; ASTM D1525
Brittleness Temperature <= -68.0 °C<= -90.4 °FASTM D746
Glass Transition Temp, Tg -46.0 °C-50.8 °FDMA
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 °C383 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5590 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
Austin Novel Materials Texalan® 585A Polyether-based TPU

PB1T10 / 26554

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.