MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retard dust and maintain their original state and color for many years.

Applications:
  • Outdoor furniture
  • Automotive
  • Appliance markets

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Filler Content 40 %ASTM D2584
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 1.59 mm
ASTM D955
Melt Flow 16 - 20 g/10 min230/2.16; May be specified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 87ASTM D785
Tensile Strength at Break 3150 psiASTM D638
Flexural Modulus 360000 psiTangent; ASTM D790
Izod Impact, Notched 0.900 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched NBAt 73°F; ASTM D256
Gardner Impact 4.00 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 235 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram RamOfin PPC365T8 Polypropylene, 40% Mineral Filled
Plastics Group Polifil® RMT-40V 40% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
LyondellBasell Moplen EP380S Polypropylene, Impact Modified; Molded/Extruded
LG Chemical LUPOL HF5254A PP+MF20%
Kraton® G1657 + PP blend + Talc (12/21/67)

PPOLI019 / 56923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.