MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
XADC-Armoloy Diamond-Chrome Composite Coating
Categories: Metal; Metal Matrix Composite; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications from plastic injection mold tooling to aerospace applications that require long life expectancy, extreme wear protection, low frictional characteristics and corrosion protection. XADC-Armoloy® will not fracture from the basis metal unless the metal substrate itself fractures or fatigues. The absolute, positive adhesion that is created with the special application of XADC-Armoloy® is a major benefit to its users.

Applied at temperatures under 200°F (100°C) there are absolutely NO changes in the basis metals that the XADC-Armoloy® coating is applied to. Like Armoloy® TDC, XADC-Armoloy® will adhere and perform well on all major ferrous and nonferrous basis materials. Aluminum, magnesium, and titanium are not considered good substrates for coating with Armoloy processes.

Information provided by Armoloy of Western Pennsylvania.

Key Words: Chrome Plating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.100 - 0.300 milRecommended range
 0.0400 - 0.700 milPossible range
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 98
Coefficient of Friction, Dynamic 0.090XADC-Armoloy® vs. XADC-Armoloy®; Sliding; No lubricants at 72°C
 0.14XADC-Armoloy® vs. Steel; Sliding; No lubricants at 72°C
Coefficient of Friction, Static 0.12vs. itself; No lubricants at 72°C
 0.15vs. Steel; No lubricants at 72°C
Taber Abrasion, mg/1000 Cycles 4.66Per Fed. Std/141
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1400 °F
Minimum Service Temperature, Air -400 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 100 °CApplication Temp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 380.0-F Die Casting Alloy
Aluminum 514.0-F, Sand Cast
Aluminum A360.0-F Die Casting Alloy
Aluminum A380.0-T5, Casting Alloy
Aluminum A413.0-F Die Casting Alloy

NARMOL00 / 15016

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.