MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES HiFill FR® PP GF10 FR BK 10% Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler; Polypropylene, Flame Retardant

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 10% Filler by Weight

Features: Flame Retardant

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccASTM D792
Water Absorption 0.010 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 5000 psiASTM D638
Elongation at Yield 2.0 %ASTM D638
Flexural Yield Strength 6000 psiASTM D790
Flexural Modulus 600000 psiASTM D790
Izod Impact, Notched 0.650 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 4.50 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Strength 500 V/milMethod A (Short-Time); ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 305 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °FUnannealed; ASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 1009 GK Polypropylene, 10% Glass Filled
Techmer ES HiFill® PP GF10 CC 10% Glass Filled
BASF Ultradur® B 4300 G4 20% Glass Filled PBT
Dow Fusabond® P613 Polymer Modifier
Dow Fusabond® E226 Polymer Modifier

PTPC0751 / 136689

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.