System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Hippe PI
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyimide, Thermoplastic
Material Notes:
Wide temperature range for use. High oxidation resistance. UV stability, low coefficient of linear expansion, good strength at high temperatures, resistance against stress cracking.
Information provided by Hippe.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.43
g/cc
DIN 53 479
Mechanical Properties
Original Value
Comments
Tensile Strength
86.0
MPa
DIN 53 455
Elongation at Break
7.5 %
DIN 53 455
Tensile Modulus
3.10
GPa
DIN 53 457
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance
1.00e+15
ohm
DIN 53 482
Dielectric Constant
3.55
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength
22.0
kV/mm
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index
0.0034
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
Thermal Properties
Original Value
Comments
CTE, linear
55.0
µm/m-°C
Thermal Conductivity
0.350
W/m-K
Maximum Service Temperature, Air
250
°C
Continuous use
Flammability, UL94
V-0
Descriptive Properties
Color
brown
Resistance to hot water, suds
resistant in some conditions
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ensinger TECASINT 8001 Polytetrafluoroethylene (PTFE) + Polyimide, 20% (PI)
Ensinger XP-133 Compression Molded PI Compound, 20% Carbon Fiber
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
Ensinger TECASINT 3012 Polyimide, Ochre Brown (PI)
PHIPPE988 / 121992
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.