MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8010 sec; ASTM D2240
Tensile Strength, Yield 42.1 MPaType I, 51 mm/min; ASTM D638
Tensile Modulus 2240 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 66.9 MPaASTM D790
Flexural Modulus 2340 MPaASTM D790
Izod Impact, Notched 530 J/m
@Temperature -10.0 °C
Injection Molded; ASTM D256A
 960 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 140 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 76.1 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
Annealed; ASTM D648
 78.9 °C
@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
Compression Molded, Annealed at 50 deg.C; ASTM D648
 77.8 °C
@Thickness 3.18 mm
Compression Molded, Annealed at 60 deg.C; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 199 - 210 °C
 
Descriptive Properties
AppearanceColors Available
FeaturesHigh Gloss
 High Impact Resistance
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesCapstock
 Construction Applications
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL1227 / 145796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.